Flowable fill, also known as Controlled Low Strength Material (CLSM), is designed to flow easily into trenches, utility excavations, and hard-to-reach spaces while requiring little or no mechanical compaction. Traditionally, achieving that flow has meant adding large amounts of water.
The problem? More water isn’t always better.
Excess water increases bleeding, segregation, settlement, and drying time. It can also make the finished material less uniform and more difficult to control.
Fritz-Pak’s Fill Flow offers a different approach. Instead of relying on extra water to improve flowability, Fill Flow generates millions of microscopic air bubbles that allow the material to flow while using significantly less water.
Why Traditional Flowable Fill Uses So Much Water
Flowable fill (also called Controlled Low Strength Material (CLSM)) requires high flowability because its primary purpose is to fill voids without mechanical compaction. Unlike structural concrete, strength is secondary—its ability to flow into every space is what makes it effective.
Here are the main reasons high flow is so important:
1. It Eliminates the Need for Compaction
Flowable fill is designed to be self-leveling and self-consolidating. In trenches, pipe bedding, and utility excavations, vibrating or mechanically compacting the material is often difficult or impossible.
A highly flowable mix:
- Flows under and around utilities
- Consolidates under its own weight
- Eliminates air pockets without vibration
2. It Fills Complex Voids
Many CLSM applications involve irregular spaces that conventional concrete cannot easily reach, such as:
- Around pipes and conduits
- Under slabs
- Behind retaining walls
- Abandoned tanks or vaults
- Utility trenches with multiple obstructions
High flow allows the material to surround these obstacles, minimizing unfilled voids.
3. It Produces Uniform Support
Voids beneath pavements or around utilities can lead to differential settlement later.
A highly flowable mix ensures the material contacts all surfaces, providing continuous support and reducing the risk of future settlement.
4. It Speeds Construction
Because the material flows into place on its own, crews spend less time:
- Spreading material
- Rodding or consolidating
- Compacting in lifts
- Working around congested utilities
This can significantly reduce labor and shorten installation time.
5. It Improves Worker Safety
Deep or narrow trenches can be hazardous for workers.
A flowable material can often be placed from the surface, reducing the need for personnel to enter the excavation for compaction or hand placement.
Why Water Isn’t the Best Way to Create Flow
Traditionally, producers increased water content to achieve the required consistency. While this improves flow, it also introduces several drawbacks:
- Excessive bleeding
- Aggregate segregation
- Increased settlement
- Longer drying times
- Reduced stability during transport and placement
A Different Way to Create Flow
Fritz-Pak’s Fill Flow changes how the mix behaves.
When added to the concrete mixer, Fill Flow produces a stable system of microscopic air bubbles throughout the mixture. These tiny bubbles act like miniature ball bearings, allowing aggregate particles to move past one another with much less internal friction.
The result is a highly flowable material without relying on excessive water.
Instead of increasing water content to improve workability, Fill Flow improves particle movement through engineered air entrainment.
Designing a CLSM Mix with Fill Flow
Every project has unique performance requirements, but the overall design philosophy changes when using Fill Flow.
Instead of continually increasing water until the desired flow is achieved:
- Design the mix using the required cementitious materials and aggregates.
- Add Fill Flow according to Fritz-Pak’s recommended dosage.
- Adjust the water content downward while maintaining the required flow characteristics.
- Verify flow using your project’s specified testing procedures.
The goal is to achieve excellent placement characteristics with the minimum amount of water necessary.
The Bottom Line
Flowability doesn’t have to come from excess water.
By generating millions of stable microscopic air bubbles, Fritz-Pak Fill Flow creates a highly workable CLSM that can be designed with significantly less water than traditional flowable fill mixes.
The result is a mix that flows where you need it, while reducing bleeding, segregation, settlement, and unnecessary water—all without sacrificing placement performance.
If you’re looking to improve the performance of your next flowable fill project, consider designing your mix around engineered flow instead of excess water.
Order Online
Ready to improve your CLSM mix design? Order Fill Flow through the online store and start producing more stable, easier-to-place flowable fill while reducing water demand.